| Product: | EPA &CARB Certified High Quality Low Permeation Rubber Fuel Line for Generators |
| Item No.: | JBD-A028 |
| Size & Shape: | ID≥Φ2.5 mm; Customized as Required. |
| Material: | FKM; FKM/ECO; FKM/ECO/AR/ECO |
| Structure: | 1 to 4-layers |
| Color: | Black |
| Application | Use for Generators, Generator Sets |
| EPA & CARB CERTIFICATE | YES. |
| Standard | SAE, YDK,HES, EX-S,ASTM and so on |
| Shipping Port | Xiamen |
| OEM/ODM | Accepted |
| Package | PE bag+Carton+Pallet |
| Payment Terms | T/T, L/C,Western Union |
| Factory | ISO/IATF16949 registered |
| Technical Teams | 30+ Years experience |
| Sample Leadtime | 7-15 days |
| Production Leadtime | 20-30 days |
SPECIFICATION
| Test Condition and Result | ||||||||||
| NO | Item | Test Condition | Basic Value | Test Value | Judge | |||||
| 1 | Burst test | Test burst pressure | ≥6.2MPa | 7MPa | OK | |||||
| 2 | Vacuum Collapse Test | 一81KPa ,15-60 seconds | OD Changing Rate,Max:-20% | -6.5% | OK | |||||
| 3 | Col Flexibility | A)、To be dry heat aged for 135℃×70Hrs,after aging,to be conditioned at -40℃×5Hrs | Fixed in the cold chamber through 180 degrees from the the centerline to a diameter of 10 times the Max OD of the hose | NOT FRACTURE, NO CRACKS, NOCHEKS, NO BREAKS |
OK | |||||
| Burst pressure ≥0.69MPa | 0.81MPa | OK | ||||||||
| B)、To be immersed in ASTM Oil No. 3 for 135℃×70H,then to be conditioned at -40℃×5Hrs | Fixed in the cold chamber through 180 degrees from the the centerline to a diameter of 10 times the Max OD of the hose | NOT FRACTURE, NO CRACKS, NOCHEKS, NO BREAKS |
OK | |||||||
| Burst pressure≥0.69MPa | 0.76MPa | OK | ||||||||
| 4 | Tensile Strength | Outer Layer ≥8MPa Midium/Inner Layer ≥5MPa |
Outer:10MPa Midium:10MPa Inner:9MPa |
OK | ||||||
| Elongation | Outer Layer ≥150% Mid/Inner Layer ≥125% |
Outer:259% Midium:296% Inner:276% |
OK | |||||||
| 5 | Dry Heat Resistance | Ater 150℃*7days being aged, Slowly straighten | Surface without cracking and carbonization | No cracking and carbonization | OK | |||||
| 6 | FUEL RESISTANCE | To be immersed in FUEL C RT*48Hr | Inner Layer:rate of volume change ≤+10% | 7% | OK | |||||
| 7 | OIL RESISTANCE | 试To be immersed in ASTM Oil 3#150℃*7Hrs | Outer Layer:Change rate of tensile strength ≤+100% | 55% | OK | |||||
| 9 | OZONE RESISTANCE | SHALL BE ACCORDANCE WITH ASTM D 1149, THE SPECIMEN SHALL BE ALLOWED TO REST IN AN OZONE-FREE FOR 23℃×24H ,AND THE MOUNTED SPECIMEN SHALL BE PLACED IN A TEST CHAMBER CONTAINING OZONE AT 100MPA×40℃,AFTER 70Hrs OF EXPOSURE | NO CRACKS (BE VISUALLY INSPECTED UNDER 7X MAGNIFICATION) |
No Cracks | OK | |||||
| 10 | ADHESION | Length 25.4mm | peel strength ≥35.6N | 75N | OK | |||||
| 11 | KINK RESISTANCE | 300MM LONG SPECIMEN,23℃×2H,BEND HOSE ALONG ITS NATURAL CURVATURE AND INSERT THE OTHER END CAREFULLY INTO THE SECOND HOLE UNTIL IT PROJECTS 63 MM OUT THE OTHER SIDE | The ball is free to pass through | The ball is free to pass through | OK | |||||
| 12 | Ethanol fuel resistance test | To be immersed in 85%FUEL D+15% absolute ethyl alcohol RT *70Hr | Inner Layer: change rate of tensile strengthMax -40% ; | -20% | OK | |||||
| Inner Layer:Change rate in elongation:Max -40%; | -28% | OK | ||||||||
| Inner Layer:Chang rate of Volume: Max 0-15% | 7% | OK | ||||||||
| 13 | OXIDIZED FUEL TEST | —Cut three tensile (D471 C#) specimens to immerse in 200ml mixture consisting of 3600 mL of ASTM Fuel “B” and 10 mL of 90% t-butyl hydroperoxide for 40℃*14 days | Inner Layer: change rate of tensile strengthMax -30% ; | -15% | OK | |||||
| Inner Layer:Change rate in elongation:Max -20%; | -12% | OK | ||||||||
| 14 | Low Permeation test | ASTM FULE C, METHODS CONFORM TO 9.1~9.2 and EPA Regulation |
≤15g/m2/day | 10.2 | OK | |||||
OEM & ODM
EPA &CARB Certified High Quality Low Permeation Rubber Fuel Line for Generatorse can be accepted OEM & OEM as per client’s drawings ,samples and other requirements, meeting the Low Permeation requirement according to the Standard of SAE, YDK,HES, EX-S,ASTM,
EPA & CARB CERTIFICATE
EPA &CARB Certified High Quality Low Permeation Rubber Fuel Line for Generatorse achieved the EPA & CARB Certificate.
APPLICATION
EPA &CARB Certified High Quality Low Permeation Rubber Fuel Line use for Generators, Generator Sets.
Product detail pictures:
Related Product Guide:
Our corporation has been specializing in brand strategy. Customers' gratification is our greatest advertising. We also source OEM company for PriceList for Airmatic Repair Kit – EPA &CARB Certified High Quality Low Permeation Rubber Fuel Line for Generators – JINBEIDE , The product will supply to all over the world, such as: San Francisco, Eindhoven, Philadelphia, We believe that good business relationships will lead to mutual benefits and improvement for both parties. We have established long-term and successful cooperative relationships with many customers through their confidence in our customized services and integrity in doing business. We also enjoy a high reputation through our good performance. Better performance will be expected as our principle of integrity. Devotion and Steadiness will remain as ever.
It is a very good, very rare business partners, looking forward to the next more perfect cooperation!
Write your message here and send it to us